How Subtera detects CUI
How does Subtera’s technology detect concealed corrosion and moisture?
Carbon steel pipework and process vessels are a similar temperature of the process fluid contained within.
Due to the electrically conductive nature of metals, uncorroded steel is a poor emitter of THz light.
When corrosion occurs, the change in molecular state from carbon steel to iron oxide, enables the iron oxide (corrosion) to radiate THz light at a greater intensity than uncorroded metal. The radiated intensity is dependent on a range of factors including temperature, specific composition, and thickness of the corrosion.
The insulation surrounding the asset is also heated through conduction, and as it is non-electrically conductive, it too radiates THz light; again, in proportion to its temperature, composition, and thickness.
THz light from corrosion and moisture, transmits through the insulation and polymeric cladding, and then it is then measured by Subtera.
Share article:
You may also like to read
Signup to our newsletter
To hear the latest from Subtera about our technology, industry insights, case studies and company news, enter your email and we’ll send updates directly to your inbox.
By signing up, you agree to our privacy policy.